Nanoindentation

Nanoindentation

Anthony C. Fischer-Cripps - Collection Mechanical Engineering Series

263 pages, parution le 04/10/2004 (2eme édition)

Résumé

There has been considerable interest in the last two decades in the mechanical characterisation of thin film systems and small volumes of material using depth-sensing indentation tests. Usually, the principal goal of such testing is to obtain values for elastic modulus and hardness of the specimen material from experimental readings of indenter load and depth of penetration. But other properties such as residual stress, fracture toughness, and visco-elas-tic behavior may also be measured. The indentation technique can be used on both brittle and ductile materials where conventional testing may result in premature specimen fracture. The forces involved are usually in the millinew-ton range and measured with a resolution of a few nanonewtons while the depths of penetration are in the order of nanometres, hence the term "nanoindentation".

This new edition of Nanoindentation includes:

  • A dedicated chapter on thin films
  • New material on dynamic analysis and creep
  • Accounts of recent research
  • Three new appendices on nonlinear least-squares fitting, frequently asked questions, and specifications tor a nanoindentation instrument.

Nanoindentation Second Edition is intended for those who are entering the field for the first time and to act as a reference for those already conversant with the technique.

L'auteur - Anthony C. Fischer-Cripps

Anthony C. Fischer-Cripps, Ph.D. is the Project Leader for Surface Mechanics, Telecommunications & Industrial Physics at Commonwealth Scientific & Industrial Research Organization in Lindfield, Sydney, Australia.

Sommaire

  • Contact Mechanics
  • Nanoindentation Testing
  • Analysis of Nanoindentation Test Data
  • Factors Affecting Nanoindentation Test Data
  • Simulation of Nanoindentation Test Data
  • Scaling Relationships in Nanoindentation
  • Methods of Nanoindentation Testing
  • Nanoindentation Test Standards
  • Nanoindentation Test Instruments Chapter
  • Examples of Nanoindentation Testing
Voir tout
Replier

Caractéristiques techniques

  PAPIER
Éditeur(s) Springer
Auteur(s) Anthony C. Fischer-Cripps
Collection Mechanical Engineering Series
Parution 04/10/2004
Édition  2eme édition
Nb. de pages 263
Format 16x 24
Couverture Relié
Poids 541g
Intérieur Noir et Blanc
EAN13 9780387220451
ISBN13 978-0-387-22045-1

Avantages Eyrolles.com

Livraison à partir de 0,01 en France métropolitaine
Paiement en ligne SÉCURISÉ
Livraison dans le monde
Retour sous 15 jours
+ d'un million et demi de livres disponibles
satisfait ou remboursé
Satisfait ou remboursé
Paiement sécurisé
modes de paiement
Paiement à l'expédition
partout dans le monde
Livraison partout dans le monde
Service clients sav.client@eyrolles.com
librairie française
Librairie française depuis 1925
Recevez nos newsletters
Vous serez régulièrement informé(e) de toutes nos actualités.
Inscription